Type: | Seamless |
---|---|
Technique: | Cold Drawn |
Material: | Carbon Steel |
Surface Treatment: | Oiled |
Usage: | Pipeline Transport, Boiler Pipe, Hydraulic/Automobile Pipe, Oil/Gas Drilling, Machinery Industry, Chemical Industry, Mining, Construction & Decoration |
Section Shape: | Round |
Fournisseurs avec des licences commerciales vérifiées
Standard & Matériel | L'acier au carbone | La norme ASTM A519 | MT1010, TM1020, 1008, 1010, 1018, 1020, 1025, 1030, 1045, 1518 |
La norme JIS G3445 | STKM11A STKM12A STKM12B STKM12C STKM13A STKM13B STKM13C STKM14A STKM14B STKM14C STKM15A STKM15C STKM16A STKM16C STKM17A STKM17C STKM18A STKM18B STKM18C STKM19A STKM19C STKM20A | ||
La norme JIS G3473 | Sc370, SC440, SC510A, SC510, SC540, SC590A, STC590B | ||
La norme DIN 2391 | St 35, ST45, ST52 | ||
La norme EN 10297-1 | E235, E275, E315, E355, E470 | ||
La norme EN 10305-1 | E215, E235, E355 | ||
La norme EN 10305-4 | E215, E235, E355 | ||
La norme BS 6323-3 | HFS 3, 4 HFS, HFS 5, HFS 8 | ||
NF A49-311 | TU 37-b, TU 52-b, TU 56-b, tu XC35 | ||
En acier allié | La norme ASTM A519 | 1345, 3140, 4130, 4135, 4140, 4150, 4320, 4340, 5120, 5130 | |
La norme JIS G3429 | STH STH2111, 12, 122 STH31 | ||
La norme JIS G3441 | La SCR420les savoirs traditionnels, SCM415les savoirs traditionnels, SCM418les savoirs traditionnels, SCM420les savoirs traditionnels, SCM430les savoirs traditionnels, SCM440LES SAVOIRS TRADITIONNELS | ||
Acier inoxydable | La norme ASTM A511 | MT304, MT304L, MT310S, MT316, MT316L, MT317, MT321, MT347, MT403, MT410, MT431 | |
La norme ISO | NACE MR-0175 | ||
Taille |
Gamme de taille | La tolérance | |
OD | 6-325mm | -- +0.045-0.035 mm | |
ID | 2-250mm | ±0.035mm | |
WT | 1-32mm | Dépend de tailles | |
Longueur | Longueur fixe ou aléatoire | +0-3.5mm | |
La linéarité | 0, 15: 1000, 0.4: 1000, 0, 5: 1000 1: 1000 ou personnalisées | ||
La rugosité de surface | Ra 0, 02-0.4μm |
Grade d'acier | C(%) | Si(%) | Mn(%) | P(%) | S(%) | Nb/V(%) |
STKM11A | ≤0, 12 | ≤0, 35 | ≤0, 60 | ≤0, 040 | ≤0, 040 | - |
STKM12A | ≤0, 20 | ≤0, 35 | ≤0, 60 | ≤0, 040 | ≤0, 040 | - |
STKM12B | ≤0, 20 | ≤0, 35 | ≤0, 60 | ≤0, 040 | ≤0, 040 | - |
STKM12C | ≤0, 20 | ≤0, 35 | ≤0, 60 | ≤0, 040 | ≤0, 040 | - |
STKM13A | ≤0, 25 | ≤0, 35 | 0.30~0.90 | ≤0, 040 | ≤0, 040 | - |
STKM13B | ≤0, 25 | ≤0, 35 | 0.30~0.90 | ≤0, 040 | ≤0, 040 | - |
STKM13C | ≤0, 25 | ≤0, 35 | 0.30~0.90 | ≤0, 040 | ≤0, 040 | - |
STKM14A | ≤0, 30 | ≤0, 35 | 0.30~1.00 | ≤0, 040 | ≤0, 040 | - |
STKM14B | ≤0, 30 | ≤0, 35 | 0.30~1.00 | ≤0, 040 | ≤0, 040 | - |
STKM14C | ≤0, 30 | ≤0, 35 | 0.30~1.00 | ≤0, 040 | ≤0, 040 | - |
STKM15A | 0.25~0.35 | ≤0, 35 | 0.30~1.00 | ≤0, 040 | ≤0, 040 | - |
STKM15C | 0.25~0.35 | ≤0, 35 | 0.30~1.00 | ≤0, 040 | ≤0, 040 | - |
Grade d'acier | Résistance à la traction(N/mm²) | Limite d'élasticité(N/mm²) |
STKM11A | ≥290 | - |
STKM12A | ≥340 | ≥175 |
STKM12B | ≥390 | ≥275 |
STKM12C | ≥470 | ≥355 |
STKM13A | ≥370 | ≥215 |
STKM13B | ≥440 | ≥305 |
STKM13C | ≥510 | ≥380 |
STKM14A | ≥410 | ≥245 |
STKM14B | ≥500 | ≥355 |
STKM14C | ≥550 | ≥410 |
STKM15A | ≥470 | ≥275 |
STKM15C | ≥580 | ≥430 |
+C(BK) | Étiré à froid/disque. Après la dernière formage à froid, aucun traitement thermique. |
+LC(BKW) | Étiré à froid/soft. Après le dernier traitement thermique suit l'étirage à froid il y a un passage de finition de lumière. |
+SR(BKS) | Étiré à froid et recuit soulagé de stress. Après le dernier processus d'étirage à froid les tubes sont soulagés recuit de stress dans une atmosphère contrôlée. |
+d'un(GBK) | Après le dernier processus d'étirage à froid les tubes sont soulagés recuit de stress dans une atmosphère contrôlée. |
+N(NBK) | Normalisée. Après le dernier processus d'étirage à froid les tubes sont recuites dans une atmosphère contrôlée. |